I would imagine you should be able to get away with the 1.5mm tip. I certainly don’t want to second guess Earlex’s technical department but it might be worth trying to thin even more, down to my previous recommendation. All you will be out is a little time and some thinner if it doesn’t work.

I don’t have much experience with high build lacquer, but the high solids count could certainly have a big affect on the viscosity and the “sprayability” of the mix. Unless you have a specific need for high build, it might be best to stick with your regular formulations in the future. Good luck and keep us posted.

-- For free video tutorials and other cool woodworking stuff, check out http://www.TheWoodWhisperer.com


DISCLAIMER: Any posts on LJ are posted by individuals acting in their own right and do not necessarily reflect the views of LJ. LJ will not be held liable for the actions of any user.

Latest Projects | Latest Blog Entries | Latest Forum Topics

HomeRefurbers.com