I use the MW Polycrylic Gloss a lot and have had best results lightly sanding with 320 grit between coats 1-2 and 2-3.

After 3rd coat I use “0000 synthetic steel wool pad and end up with somewhere between gloss and satin finish. On large flat surfaces I use a sanding pad with rubber face with the synthetic steel wool pad to make a uniform pass and with very little pressure.

-- Rick Gustafson - Lost Creek Ranch - Colorado County, Texas